Moisture and Air · Gaseous Contamination

Corrosive Gases and Electronics: Why Sulfur, Humidity and Lead Free Solder Add Up to Hardware Failures

Corrosive gases are sulfur, chlorine and other compounds in the air that react with copper and silver in electronics, forming films that break circuits or short them.

When electronics moved to lead free solders and finishes under the EU RoHS directive, industry groups began reporting a corrosion mode called creep corrosion. Corrosion products spread across circuit boards and short them out.

The air in a data hall can look perfectly clean and still be slowly eating copper and silver on every board. Humidity speeds it up, and most sites never measure it.

Key takeaways

  • Sulfur bearing gases, chlorine compounds, nitrogen oxides and ozone attack copper and silver on boards, connectors and components.
  • ASHRAE recommends ISA 71.04 severity level G1: copper reactivity below 300 angstroms per month and silver below 200 angstroms per month.
  • Copper and silver coupons left in the airstream for about 30 days measure how corrosive the air is. A walk past cannot.
  • Humidity multiplies the damage. ASHRAE's 5th edition allows 70% relative humidity only where coupons show low gas levels.

What are corrosive gases, and where do they come from?

Corrosive gases are trace gases in the air that react with metals. In data halls, the ones that matter most are a short list.

  • Sulfur bearing gases, such as hydrogen sulfide and sulfur dioxide.
  • Chlorine compounds.
  • Nitrogen oxides.
  • Ozone.

Sources

Outside air near industry, wastewater treatment plants, busy roads and diesel generators carries these gases. Some building materials, cleaning chemicals and even rubber products give off sulfur compounds indoors.

Airside economizers bring outside air, and its contaminants, straight into the hall. Particle filters stop dust but do nothing for gases, as covered in Part 6.

The concentrations involved are tiny, often parts per billion. That is why they go unnoticed: no smell, no haze, no visible dust. The damage shows up on hardware months or years later.


How do corrosive gases damage electronics?

Corrosive gases react with copper and silver on circuit boards, connectors and components. They form thin sulfide and oxide films on the metal surface.

Three ways it causes failures

  • Films raise contact resistance on connectors and switches, causing intermittent faults.
  • Corrosion eats through thin traces and plating, creating open circuits.
  • Corrosion products spread across the board and bridge between conductors, creating shorts.

Silver is especially vulnerable to sulfur. Silver sulfide grows quickly and can form whiskers or creep across surfaces.

The failures are hard to diagnose. A server with corroded connectors may throw intermittent errors, reboot unexpectedly or fail a component that tests fine on the bench once cleaned. Without measurement, these failures are easily blamed on bad batches or bad luck.


What is creep corrosion, and why did lead free electronics make it worse?

Creep corrosion is corrosion product, usually copper sulfide, that grows outward from exposed copper and spreads across the surface of a circuit board. When it bridges two conductors, it creates a short.

The lead free link

The EU RoHS directive restricted lead and other substances in electronics. Manufacturers moved to lead free solders and new surface finishes on circuit boards. Some of those finishes leave more copper exposed, or protect it less well in sulfur rich air.

After the transition, industry bodies including iNEMI, the International Electronics Manufacturing Initiative, highlighted creep corrosion as a growing reliability risk for lead free hardware (iNEMI via Purafil).

The result is that hardware built today can be more sensitive to air quality than hardware built two decades ago. Air that older equipment tolerated may now cause failures.


What is ISA 71.04 severity level G1?

ANSI/ISA 71.04-1985 classifies how corrosive an environment is for electronics, from mild to severe. The levels are G1, G2, G3 and GX.

G1 is the mildest level, where corrosion is not expected to affect equipment reliability. G2 is moderate, G3 harsh and GX severe.

The classification is based on how fast a corrosion film grows on copper exposed to the air, measured in angstroms per month. An angstrom is one ten billionth of a meter.

ISA is the International Society of Automation. The standard dates from 1985, but it is still the reference that data center guidance points to.


What corrosion rates does ASHRAE recommend for data centers?

ASHRAE recommends that data centers maintain ISA 71.04 severity level G1 (Teradata site planning guide). In practice that means two limits.

  • Copper reactivity rate below 300 angstroms per month.
  • Silver reactivity rate below 200 angstroms per month, an added ASHRAE criterion.

ASHRAE is the American Society of Heating, Refrigerating and Air Conditioning Engineers. It added the silver limit because silver is more sensitive to some sulfur compounds than copper, and a copper only test can miss them.

These limits apply to the air in the data hall, measured where the equipment breathes. A site that meets G1 at the intake louver but not in the hall has an indoor source.


How are corrosion coupons used to measure air corrosivity?

Corrosion coupons are small strips of pure copper and silver, cleaned and sealed in a package until use. They are placed in the airstream for about 30 days, then sent to a lab, which measures the thickness of the corrosion film that grew on them.

Placement

Vendors specify placement about 2 inches (51 mm) in front of the rack on the air inlet side, at one quarter and three quarter frame height (IBM). That measures the air the equipment actually breathes.

Coupons placed on a wall or near a computer room air handler (CRAH) return measure something else. Placement should be recorded so later tests can be compared.

Real time monitors

Real time corrosion monitors measure the same thing continuously and electronically. They show when corrosion happens, such as during a generator test or a nearby industrial release, which a 30 day coupon averages out.

Either way, this is the only reliable way to know the corrosivity class. Smell, visual checks and particle counts cannot tell you.


How do you read a coupon test report?

A coupon report usually gives a copper rate, a silver rate and a severity class. Each tells you something different.

Copper rate

The copper rate, in angstroms per 30 days, sets the ISA 71.04 class. Below 300 is G1, and 300 to 1,000 is G2.

From 1,000 to 2,000 is G3. Anything above 2,000 is GX, the severe class.

Silver rate

The silver rate catches sulfur compounds that copper can miss. ASHRAE wants it below 200 angstroms per month. A site can pass on copper and fail on silver.

Film breakdown

Many labs break the film into types, such as copper sulfide, copper oxide and silver chloride. The type points to the gas. Sulfide points to sulfur sources. Chloride points to chlorine, often from cleaning products, water treatment or coastal air.

Keep every report with the coupon location, the dates and the humidity during exposure. A number without context cannot be compared next year.


How often should a site test for corrosive gases?

There is no single required interval. Most programs follow a simple pattern.

  • A baseline survey when the hall is commissioned, or now if it never had one.
  • A repeat test once a year, at the same locations.
  • A new test after any change to outside air use, filtration or nearby land use.
  • A new test when hardware failures start to cluster.

Seasonal changes matter. Wind direction, heating season and nearby industrial activity all shift gas levels. A summer test and a winter test can tell different stories.

Sites near known pollution sources, or running economizers for much of the year, often move to continuous monitoring. It turns a yearly snapshot into a running record.


How does humidity make gaseous corrosion worse?

Humidity makes gaseous corrosion worse in two ways: it wets dust, and it gives gases water to dissolve into.

Wet dust

Dust absorbs water from the air. At a certain humidity, called its deliquescent relative humidity, the dust becomes damp enough to conduct electricity and hold corrosive ions against the metal. Equipment vendors specify that the deliquescent RH of dust in the hall should be above 60% (IBM).

Acid films

In high pollutant environments, humidity above about 50% RH helps gases form corrosive acids on surfaces (Computer Weekly). A thin film of water on a board is enough.

So humidity and gases are not separate risks. Each makes the other worse. Humidity ranges in general are covered in humidity sensing: why too dry and too wet both break things.



What other environmental conditions raise corrosion risk?

Several conditions raise corrosion risk even where gas levels are moderate.

  • High humidity, especially sustained above 60% RH.
  • Temperature swings that cause condensation on equipment, covered in Part 1.
  • Outside air brought in without gas phase filtration.
  • Nearby battery rooms or generator exhaust.
  • Dust that holds moisture.

Gas phase filtration

Gas phase filters use chemical media to absorb or react with corrosive gases. Sites with economizers or nearby pollution sources often need them on outside air units. Particle filters alone do nothing for gases.

Raised floor plenums and ceiling voids can also collect gases and dust from other spaces. Check where return air actually comes from before assuming it is clean hall air.

Battery rooms and generators deserve attention. Battery off gassing and diesel exhaust can carry sulfur and acid compounds into adjacent spaces. Gas sensing near battery rooms is covered in VOC and gas sensing.


What can you see before coupons are tested?

Visual clues exist, but they come late. By the time corrosion is visible, it has already happened.

  • Blackened or discolored copper on exposed busbars, connectors and cable lugs.
  • Tarnished silver plated contacts.
  • Dark films on copper pipe or fittings in the hall or nearby rooms.

Routine visual inspection of exposed copper in electrical rooms and data halls, photographed the same way each time, shows whether tarnish is spreading. A change in color over months is a reason to test, not a reason to wait.

Particle related failures, such as zinc whiskers from older raised floor tiles, are a separate issue covered in particulate and air quality in data centers.


What looks like gaseous corrosion but is not?

Three conditions look like gas corrosion.

Normal oxidation

Decorative or structural copper that has no electrical role darkens over time in any air. It is not a reliability finding on its own.

Heat discoloration

Overloaded or loose connections discolor from heat, not chemistry. The pattern is local to one connection. Electrical heating is covered in the Electrical, Controls and Safety series and in thermal imaging.

Particulate failures

Zinc whiskers and conductive dust cause shorts too, but by a different mechanism. They are covered in the existing particulate post.


What does corrosive air cost?

Corrosive air costs hardware, diagnosis time and operating flexibility.

In an office building

Corrosion of controls, building management system panels and electrical connections in rooms near outside air intakes or exhaust sources.

In a data center

Intermittent hardware failures. Connector and board failures that are hard to diagnose. Loss of the right to operate at higher humidity under ASHRAE guidance, which costs energy.

Warranty and vendor disputes

Many hardware vendors list gaseous contamination limits in their site requirements. When boards fail early, a vendor may ask for coupon data before honoring a claim. A site with no data has little to argue with.

Hidden cost of guessing

Without measurement, teams often replace hardware, swap power supplies or blame firmware. Each step costs time and parts. A coupon survey usually costs far less than one failed server, and it can end months of chasing faults.

The opposite mistake is just as costly. A site with clean air that never tests must run at tighter humidity limits than it needs. That means more humidifier and dehumidifier energy every hour of the year.


What do you do when a site fails G1?

A failed coupon test is a starting point, not a verdict. The fix depends on where the gas comes from.

Find the source

Compare coupons at the outside air intake, in the supply air and at the rack inlet. If the intake is worst, the source is outside. If the hall is worse than the intake, the source is inside.

Outside sources

Add or upgrade gas phase filtration on outside air units. Reduce economizer hours during known pollution events, such as generator tests or nearby plant releases. Check that intakes are not close to exhausts or loading docks.

Inside sources

Look for cleaning chemicals, rubber flooring, new construction materials and battery off gassing. Seal paths from battery rooms and generator spaces into the hall.

Control humidity

Keep relative humidity lower while the source is fixed. This slows the damage even if gas levels stay the same for a while.

Retest

Repeat the coupon test at the same spots after each change. That shows which change worked and gives the record a closing entry.


What can a walk past prove, and what needs a follow up test?

A walk past can find the conditions that raise risk and the late visual signs. It cannot measure corrosivity.

Directly observable

Tarnish and blackening on exposed copper and silver. Outside air sources near intakes. Humidity readings.

Strong indicators

Humidity regularly above 60% in a site with economizers or nearby pollution sources. Repeated unexplained hardware failures concentrated in one area.

Suspected, needs follow up

The actual corrosivity class. That needs copper and silver reactivity coupons or a real time corrosion monitor.

Logging humidity, nearby sources and copper condition on every round builds the case for testing, and later shows whether filtration and humidity changes worked. No single sensor answers this question alone.


Walk up checklist for corrosive gases

  • Temperature and humidity in data halls and electrical rooms.
  • Exposed copper busbars, lugs and connectors for blackening.
  • Outside air intakes and nearby pollution sources such as generators, loading docks and treatment plants.
  • Gas phase filtration on outside air units, installed or not.
  • Last coupon test: date and result.

How FacilityOps detects it

Coming Soon


Questions to ask about your own equipment

  1. 1. Have you ever measured your data hall's corrosivity with copper and silver coupons?
  2. 2. Does your site use outside air, and is it filtered for gases?
  3. 3. What humidity limit do you operate to, and can you justify it with coupon data?
  4. 4. What pollution sources sit near your air intakes?
  5. 5. Do hardware failures cluster in any part of the hall?

Frequently asked questions about corrosive gases and electronics

What corrosive gases affect data centers?

Mainly sulfur bearing gases such as hydrogen sulfide and sulfur dioxide, chlorine compounds, nitrogen oxides and ozone.

What is ISA 71.04 G1?

G1 is the mildest corrosivity level in ANSI/ISA 71.04-1985, where corrosion is not expected to affect equipment reliability. ASHRAE recommends data centers maintain it.

What copper and silver corrosion rates does ASHRAE recommend?

Copper below 300 angstroms per month and silver below 200 angstroms per month, measured with reactivity coupons.

What is a corrosion coupon?

A small strip of pure copper or silver placed in the airstream for about 30 days. A lab measures the corrosion film that grows on it to classify the air.

What is creep corrosion?

Corrosion product, usually copper sulfide, that spreads across a circuit board from exposed copper and can short adjacent conductors.

Did lead free electronics increase corrosion risk?

Industry bodies including iNEMI highlighted creep corrosion as a growing risk for lead free hardware after the EU RoHS restrictions.

How does humidity affect gaseous corrosion?

Humidity wets dust so it conducts, and above about 50% RH in polluted air it helps gases form corrosive acids on surfaces.

Can a data center run at 70% humidity?

ASHRAE's 5th edition allows a 70% RH upper limit only where coupon measurements show low pollutant gas levels. Otherwise lower limits apply.

Do airside economizers increase corrosion risk?

They can, because they bring outside air and its gases straight into the hall. Gas phase filtration and coupon testing manage the risk.



Sources


Everything in this piece, as a checklist you can take on your rounds

Turn the key points from this article into a practical inspection checklist.